A cikin tsarin amfani aluminum composite panels, idan akwai matsala ta blister a saman fale-falen.
menene dalilin hakan? Za mu iya gano dagaaluminum composite panel masana'anta.

Yana yiwuwa cewa core farantin extrusion da granular wadanda ba fusible abu,
Matsakaicin diamita na waɗannan abubuwan da ba su da ƙarfi zuwa wani ɗan lokaci, za su fito daga saman farantin ɗin,
da hadadden zai haifar da farantin surface kumfa sabon abu.
Lokacin da muka kware dagaaluminum-plastic farantin za a ga cewa akwai alamun rashin haɗin gwiwa a kusa da bulge,
dalilin wannan alamar shine kumburin yana cikin mahallin latsawa,
Ba za a iya fitar da iskan da ke kusa da ɓangaren ɓoyayyen ɓoyayyen ɓoyayyiyar ƙwanƙwasa ba kuma a yi sandwiched a tsakiyar layin farantin.
siraran iskan ya toshe cikakken mannewar Layer Layer zuwa.
Wadannan abubuwan da ba su narke ba na iya zama barbashi na robobi da aka gauraya su cikin wasu kazanta, za a iya samun wasu barbashi na roba da aka gauraye a ciki.
wurin narkewar waɗannan robobi ya fi polyethylene girma,
a cikin dunƙule ganga ba zai iya narke kuma an katange a cikin bakin karfe waya raga sheet gefe,
idan aka tattara zuwa wani wuri zai haifar da extrusion baya matsa lamba.
ta yadda saman ya karya allon tare da extrusion lalacewa ta hanyar core farantin kumfa.

Idan girman barbashin wanda bai narke ya yi yawa ba, yana iya makale a baki ya mutu.
don haka saman allon ɓangarorin da aka fitar ya zama alamomi masu zurfi.
wanda kuma zai haifar da matsala masu inganci a samanaluminum-plastic allo.