Akwai matakai daban-daban na samarwa na aluminum composite panel, wanda za a iya raba zuwa sanyi hadadden hanya da zafi hadaddun hanya bisa ga hadadden tsari na filastik core panel da biyu-gefe aluminum panel; Hakanan za'a iya raba shi zuwa hanyar haɗaɗɗiyar ci gaba da hanyar haɗaɗɗiyar tsaka-tsaki. Tsarin farko na samar da panel composite aluminum shine tsaftacewa na aluminum. Aluminum coil a cikin samar da tsari saboda bukatar, an rufe saman da man shafawa da kuma anti-oxidants, a cikin sufuri kuma za a haɗe zuwa wani datti, wadannan za su shafi da bonding, don haka dole ne a tsaftace shi. Aluminum nada bayan tsaftacewa da kuma sinadaran magani, da surface zai samar da wani Layer na m sinadaran kariya film; wannan Layer na fim din sinadarai na iya inganta juriya ga oxidation na aluminum coil da kuma tsawaita rayuwar fim din fenti.
Babban tsari na tsaftacewa shine kamar haka.
Aluminum coil → spraying degreasing → wanke ruwa → neutralization → maganin sinadarai → wanke ruwa → bushewa → sanyaya → iska.
Ana ciyar da coil ɗin alumini mai tsabta a cikin injin ɗin da ke rufewa don ɗaukar saman saman kwal ɗin aluminium tare da babban aiki na fluorocarbon guduro.
Tsarin tsari shine kamar haka.
Aluminum coil → ciyarwa → shafi fluorocarbon shafi → zafi iska wurare dabam dabam yin burodi → sanyaya → laminating → yankan → rewinding.
Za a lulluɓe bangarorin fale-falen fale-falen aluminium na waje tare da manyan riguna guda biyu da firam ɗin kowanne. Babban gashin bangon bangon waje shine flUorocarbon resin shafi tare da matsanancin juriya na yanayi, wato polyvinylidene fluoride (PVDF), wanda mafi kyawun juriya na UV da juriya ga gurɓataccen muhalli ya sa saman murfin aluminium mai kariya ya kula da launi mai haske. Fuskar aluminum composite panel ba zai iya samun launi na karfe kawai ba, amma har ma da kyakkyawan tsarin marmara da launi. Ana amfani da murfin Fluorocarbon akan na'urar aluminium ta hanyar abin nadi, sannan a gasa shi da zafi mai zafi don bushewa. Kayan aiki yana ci gaba da samarwa, tare da kayan shafa na farko, sa'an nan kuma saman shafi, kuma a ƙarshe surface varnish. Jimlar kaurin fenti guda uku ya kai 30μm, kuma kowane fenti yana buƙatar toya sama da 200 ℃ na kimanin 60s don bushewa, sannan a sanyaya cikin sauri ta hanyar sanyaya iska bayan barin tanda. Epoxy guduro, polyester guduro da acrylic guduro za a iya amfani da ciki bango panel fenti. Bayan na farko, saman gashi da kuma saman varnish an rufe su, an yi amfani da fim ɗin kariya na PE nan da nan a kan saman rufin rufin don kauce wa lalacewa a lokacin aiki na gaba da kuma jigilar sufuri da shigarwa.
Fim ɗin mai kariya yana ɗaukar kansa kuma ana iya cire shi bayan shigarwa. Gilashin aluminium wanda aka lullube shi da resin fluorocarbon zai iya shigar da tsarin lamination tare da ainihin kayan filastik. Ƙaƙwalwar filastik shine ainihin yadudduka uku, tare da filastik PE a tsakiya da kuma m a bangarorin biyu, kuma za a iya samar da takardar PE da adhesive daban ko a cikin tsarin haɗin gwiwa na Layer uku. Tsarin manne / PE / adhesive uku-Layer co-extruded takardar da aka samar da farko, sa'an nan kuma hade tare da babba da ƙananan yadudduka biyu na aluminum takardar, da hadaddun aluminum-plastic takardar hadaddun takardar ne 0.15mm kauri aluminum takardar a bangarorin biyu. , ainihin Layer shine 3-5mm, kuma jimlar kauri shine 4-6mm. a ƙarshe, an yanke takardar zuwa girman 1220mm × 2440mm.